Our Location
Zhejiang,China
1.Handmade
2.High temperature refractory material.
3.Smelting ZnO crucible with purity of more than 99.5%
1. Indirect smelting of ZnO.
2.No easy to deform.
3.No easy to crack.
4. Anti-ZnO liquid erosion.
| Items | Unit | Enterprise standard | Directions |
|---|---|---|---|
| Ai203 | % | ≥29.6 | |
| Si02 | % | ≥67.2 | |
| Fe203 | % | ≤0.64 | |
| Apparent Porosity | % | <32 | firing till 900℃ |
| Cold compressive Strength | kg/cm2 | >80 | firing till 900℃ |
| Operating temperature | ℃ | ≥1550 | The furnace core temperature |
*If you would like to know about other clay recipes, please feel free to contact us!